A Parviainen, J Perala, L Frisk…
2009 European …, 2009
ieeexplore.ieee.org
In this study a salt spray test was used to compare the reliability of electrical connectors from two different manufacturers. The difference between connectors was in the coating materials of the connector pins. Manufacturer A used tin for the outermost coating layer, nickel for the second layer, and brass for the pin material. Manufacturer B also used tin for the outermost coating and brass for the pin material, but copper for the second coating layer. The test was executed according to SFS-ISO standard. The connectors were placed in a salt spray test …